aging

Home Aging and curing will make the profiles has better physical strength and hardness aging stove will keep the temperature at about 300 degree for hours
saw cutting

Home cut the aluminum profiles at the demanded length at 3m, 5.8m or 6mhttps://www.intop-alu.com/wp-content/uploads/2023/05/VID_20240418_164826.mp4 many aluminum chips when cutting profiles
stretching

Home stretching machine clamp the aluminum profile end then pull at a pressure stretching is a necessary process to pull the profile straight
extrusion

Home shear the log for the extrusionhttps://www.intop-alu.com/wp-content/uploads/2023/05/VID_20240418_164223.mp4 extrusion machine supply the pressure and force the liquid aluminum going through the mould profiles come out from the output, the puller will take it to the other end of the table move the profiles waiting for stretching
die making

Home cutting the TC into round pieces for turning.https://www.intop-alu.com/wp-content/uploads/2023/05/video_1714029178.mp4 after milling and electrical spark cutting, moulds are almost ready for fine abrasions dies are ready for getting more hardness and acurate tolerance.
log making

Home aluminum liquid flow through the channel to the mould area high pressure water to lower the temperature down and solidify the aluminum aluminum logs are cut into the demanded lengths then for Homogenizing
casting

Home casting is to melt the aluminum ingot to make the aluminum log, in order to get better log element content, refining is necessary. casting need to wear protection masks and stand at a distant place.
aluminum ingot

Home aluminum ingot is the aluminum content >99%, some are even higher.https://www.intop-alu.com/wp-content/uploads/2023/05/video_1714029899.mp4